ISO Workpiece Material Groups P, M, K, N, S, H: Matching the Insert Grade to the Material
Steel, stainless, cast iron, aluminium, titanium, hardened steel — the ISO material groups decide which insert grade to quote first. How to read the letters and the grade numbers before you order.
ISO Workpiece Material Groups P, M, K, N, S, H: Matching the Insert Grade to the Material
Start with the material, not the insert
The first question in any insert quotation is not the price. It is what the customer cuts. A grade that runs well in plain carbon steel can fail in stainless, and a grade built for cast iron will not survive a nickel alloy. The cutting-tool industry answers that question with one shared language: the ISO workpiece material groups, six letters from P to H. Every insert grade is built for one of those letters first, and the number after the letter second. Read the letters and the numbers before you order, and the quotation starts from the right grade family instead of from a guess.
The six groups at a glance
P — Steel. Plain carbon steels such as 1045, alloy steels such as 4140 and 4340, and tool steels such as A2 and D2. The most common group in general machining, and the widest range: from free-machining steels below 240 HB up to hardened tool steels at 45 HRC and tensile strengths toward 1450 MPa. Most turning and milling inserts a distributor sells are P grades.
M — Stainless steel. Ferritic, martensitic (410, 420), austenitic (304, 316), duplex (2205) and precipitation-hardening grades (17-4PH). Stainless work-hardens and holds heat at the edge, so M grades are built for that heat and that work-hardening rather than for the hardness alone.
K — Cast iron. Grey iron (GG25), ductile iron (GGG40), malleable iron and compacted graphite iron. Cast iron is abrasive and the cut is often interrupted, so K grades are built for wear resistance and edge strength at the same time.
N — Non-ferrous metals. Wrought and cast aluminium alloys (AlMgSi, AlCuMg), copper alloys, graphite and polymers. Soft, often gummy materials where the insert needs a sharp edge and a polished surface more than it needs hardness.
S — Heat-resistant alloys. Titanium and titanium alloys (Ti-6Al-4V), nickel-based superalloys (Inconel 718, Waspaloy), iron-based alloys (A-286) and cobalt-based alloys (Haynes 25, Stellite). Low thermal conductivity puts the heat into the tool, so S grades are built to survive heat that would destroy a P grade in minutes.
H — Hardened materials. Hardened steels above 45 HRC and chilled or hardened cast iron. Hard turning and hard milling, where the insert meets material that is already harder than most steels.
Hardness and tensile-strength ranges above are the ISO group ranges from the standard workpiece-material table. A single material grade sits inside one group and one sub-group — 304 stainless is an austenitic M3, Ti-6Al-4V is an S1 — so send the material grade with the enquiry and the group follows from it.
Grade numbers: 05 to 30
The letter says which material the grade is for. The number after it says what kind of cut it is for. Each group runs from 05 to 30 in steps of five, and the rule is the same in every group.
A low number — 05 or 10 — is a hard, wear-resistant grade. It holds its edge at high cutting speeds and gives the best surface finish, so it is the choice for finishing and for continuous cutting, where the edge stays in the cut.
A high number — 25 or 30 — is a tough grade. It resists edge chipping and breakage, so it is the choice for roughing and for interrupted cutting, where the edge enters and leaves the material and takes the shock each time.
The same letter with a different number is a different tool. P05 finishes steel; P30 roughs it. Pick the letter for the material first, then the number for the operation — finishing or roughing, continuous or interrupted — and the grade is decided by the job, not by habit.
Using the two together in a quotation
A distributor who quotes by the ISO groups needs four facts from the customer, and they are the same four facts our product team asks for on every grade enquiry.
- What material grade are you cutting? 1045, 304, GG25, Ti-6Al-4V — the grade gives the ISO group directly.
- How hard is it? Hardness in HB or HRC places the material inside its group and rules out grades that are too soft or too brittle for it.
- Finishing or roughing? Finishing takes a low grade number; roughing takes a high one.
- Continuous or interrupted cut? An interrupted cut needs toughness, so the grade number moves up even when the material stays the same.
Send those four lines to info@cutstars.com or WhatsApp +86-151 1148 8179 and we will return the grade that fits the material and the operation, with a trial quantity to prove it on the customer's own machine. Distributors and importers can request the catalogue the same way. Enquiries are accepted by WhatsApp, the website form and email.
Where CutStars grades fit
CutStars grades follow the same letters. Our P-group steel turning grades run CS154C, CS254C and CS354C, from finishing to heavy roughing, and our cermet grades cover finishing work in steel.
Grades for stainless, cast iron, titanium and heat-resistant alloys are quoted the same way — by material group and by operation — so send the material grade and the four facts above and we will match the grade before quoting a price.